What You Need to Know About Paint Storage & Use for Your Finishing Operation

What You Need to Know About Paint Storage & Use for Your Finishing Operation

Most paints used in finishing operations are classified as either a flammable or combustible liquid. Under certain conditions, these liquids can produce vapors that may ignite, causing a fire or deflagration.

That is why codes and standards outlining proper storage guidelines have been developed to minimize risks and protect your workers, equipment and facility. Understanding these codes and standards is key when storing, dispensing or mixing paint and selecting the right type of enclosure for your needs.

Adding a Paint Mix Room or Hazardous Material Storage Building  enables you to dispense or mix paint in a clean, ventilated environment, reducing the chance of contamination in your paint job.

It is important to understand the characteristics of the paints used in your operation; Safety Data Sheets (SDS) provide key information. You also should know the answers to the following commonly asked questions before investing in an enclosure for paint storage or to contain a mixing, dispensing or pumping process:

1. How Much Paint Can I Store or Have in Use in My Facility?

The amount of paint you can store or have in use in your facility is dependent on which class of liquid your paint falls within and the Maximum Allowable Quantity (MAQ) — the limit on the amount of flammable or combustible liquid present before additional measures are required to mitigate the hazard. The MAQ not only varies based upon the class of the liquid, but also whether the container is open or closed. The MAQ values can be found in NFPA 30, NFPA 33 and the International Fire Code (IFC). The table below is a summary of information contained in the IFC:

If your building is equipped with an automatic sprinkler system, the MAQ for storage and use can be increased by 100 percent. The amount in storage can be increased by another 100 percent (for a total increase of 200 percent) if stored in an exhausted enclosure, such as a mix room or Hazardous Material Storage Building.

 2. When Do I Need a Mix Room or Hazardous Material Storage Building?

When transferring paint between containers or mixing liquids into one container, code requires you to perform these operations in a mix room or in a spray booth with the ventilation on. Since mixing paint in a spray booth dramatically slows down your finishing operation, having a dedicated space such as a mix room is ideal.

If the amount of paint stored in your facility is over the MAQ, including the increases for ventilated enclosures and fire protection systems, a Hazardous Material Storage Building is your best option. With a fire-rated ceiling and walls, a Hazardous Material Storage Building creates a separate control area — an area protected from fire — from the rest of your facility.

NFPA 33 sets limits on how much liquid can be in a mix room, depending on its proximity to a spray booth. If a mix room is located adjacent to or within 6 feet of a spray booth, the combined amount of liquid in the mix room and the spray booth cannot exceed 120 gallons or 2 gallons per square foot of the mix room (whichever is less); the maximum amount of liquid permitted in a spray booth is 60 gallons. For mix rooms located more than 6 feet from a spray booth, the amount of paint in the mix room cannot exceed 2 gallons per square foot, regardless of the class of the liquid.

3. How Many Mix Rooms or Hazardous Material Storage Buildings Can I Have in My Facility?

There is no limit on the number of mix rooms or Hazardous Material Storage Buildings allowed in one facility. However, a mix room cannot exceed 150 square feet, and no more than 300 gallons of flammable or combustible liquids may be stored among all your mix rooms combined, as they do not qualify as control areas since they are not constructed to have a fire rating.

4. What Are the Ventilation Requirements for Mix Rooms and Hazardous Material Storage Buildings?

When vapors are present, the minimum ventilation required for a mix room is 150 cubic feet per minute (CFM). Recent changes to NFPA 33 state that ventilation is required only when you have open Class I, Class II or Class III liquids at temperatures at or above their flash points. Class IA and IB liquids have a flash point below 73 degrees Fahrenheit, meaning ventilation is still required, as interior temperatures will likely exceed the flash point.

For Hazardous Material Storage Buildings, mechanical ventilation systems are required only for locations where Class I liquids are dispensed, according to NFPA 30. However, the IFC requires ventilation where paint quantities have exceeded the MAQ. For both codes, the ventilation rate is 1 CFM per square foot of floor area but not less than 150 CFM.

5. What Are the Electrical Area Classifications of Mix Rooms and Hazardous Material Storage Buildings?

The electrical area classification of a mix room used to be Class I, Division 1 throughout — the same as a paint booth. The revised standard allows you to apply the guidelines in NFPA 30 to establish potentially different area classifications. While there may be some cost advantages to this approach, any changes require a re-evaluation of the area classification and may result in modifications to the wiring or the location of electrical equipment.

The location of vapor sources is the determining factor for the electrical area classification of Hazardous Material Storage Buildings. Larger Hazardous Material Storage Buildings often have more space between vapor sources. As with mix rooms, NFPA 30 guidelines can be applied to establish the area classifications in a Hazardous Material Storage Building.

6. Does My Facility Need an Explosion Control Method for a Hazardous Material Storage Building?

The IFC requires an explosion control method if you have exceeded the MAQ for storage or use of Class IA liquids or the MAQ for open use or dispensing of Class IB liquids. Explosion control is not required for Class IC liquids, Class II liquids or Class III liquids, nor for closed-use systems involving Class IB liquids.

When explosion control is required, deflagration (explosion) venting is the most common option. If the Hazardous Material Storage Building is indoors, it must be placed along an exterior wall, where the deflagration vent panels line up with penetrations in the building wall to allow for exterior venting.

Another option to achieve explosion control is deflagration prevention through concentration reduction. A hazard analysis must be performed to determine if any additional airflow is needed to reduce the concentration of flammable vapors present during a spill or other accidental release of the materials. Frequent maintenance and calibration of the equipment is also required to ensure the system continues to provide the necessary level of protection.


By purchasing a mix room or Hazardous Material Storage Building from a manufacturer with a vast and experienced distribution network, such as GFS, you have a helping hand in navigating code compliance. GFS distributors are well-versed in the latest versions of NFPA 30, NFPA 33 and the IFC, as well as state and municipal regulations, and are also comfortable working with building inspectors to achieve code compliance.

WANT TO LEARN MORE ABOUT OUR PRODUCTS?

Let us know your product requirements, and we will put you in touch with a distributor in your area.

RELATED POSTS
News

Top 5 Blog Posts of 2023

As we look forward to what 2024 has in store, we pause to look back on 2023. In case you missed them, here are our top five blog posts of 2023.

Read More »
Automotive Refinish

GFS at SEMA 2023: Edge Up Your Paint Shop

GFS is excited to return to the SEMA Show to meet with body shop owners, managers, technicians and automotive refinish professionals. Visit GFS Booth #31067 from Oct. 31 to Nov. 3, 2023 in Las Vegas to learn how GFS can enable your shop to be more productive, efficient and profitable, while achieving flawless paint finishes.

Read More »
Automotive Refinish

Excellence Reimagined: New Auto Refinish Paint Booth From Global Finishing Solutions Introduced to Market

GFS is proud to introduce the Edge Paint Booth, which provides industry-leading features with an updated, modern design, while being backed by a manufacturer with decades of experience in the automotive refinish industry. Masterfully designed for today’s collision repair centers and paint shops, GFS Edge delivers advanced controls; precise, adjustable lighting; and premium contamination control to consistently produce excellent paint finishes and improved throughput.

Read More »
Automotive Refinish

Ultra XS Paint Booth a “Wow Factor” for Ministry Helping At-Risk Teens

Targeting junior high and high school students, the Crossover Restoration Foundation aims to provide an avenue for at-risk teenagers to turn around their lives. The past seven years, JB Baldridge has worked to get the ministry up and running. He finally is nearing that point, thanks to the addition of an Ultra XS Paint Booth from GFS.

Read More »
Automotive Refinish

“Potential is There for More Throughput” with Dual-Bay CTOF Booth at ABRA Faribault

With a shop expansion underway at ABRA Faribault, three things were priorities for body shop general manager Aaron Kasparek — increased flexibility, more space and better contamination control. Check, check and check, mostly thanks to a dual-bay Ultra XD Closed-Top Open-Front (CTOF) Booth from GFS that was paired with an Ultra XD Paint Booth and Ultra XD Paint Mix Room in hopes maximized productivity boosts the bottom line.

Read More »

Newsletter Signup

Global Finishing Solutions will use the information you provide on this form to be in touch with you and to provide updates and marketing. You can change your mind at any time by clicking the unsubscribe link in the footer of any email you receive from us, or by contacting us at info@globalfinishing.com. We will treat your information with respect. For more information about our privacy practices please visit our privacy policy. By clicking below, you agree that we may process your information in accordance with these terms.